Plastoplan Polska Sp. z o.o.
Polyethylene PE, LDPE, HDPE..., Polypropylene PP, Styrene copolymers ABS, SAN, ASA..., Polyamide PA, Polyacetals POM
Poland, 03-901 Warszawa, Al. Księcia Józefa Poniatowskiego 1ABS LG HI121H, granulate, natural
available quantity 16 tons
Physical |
Nominal Value
|
Unit
|
Test Method
|
Density / Specific Gravity 2
|
1/05
|
g/cm³
|
ASTM D792 |
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg)
|
22
|
g/10 min
|
ASTM D1238 |
Molding Shrinkage - Flow (23°C, 3.20 mm, Injection Molded)
|
0.40 to 0.70
|
%
|
ASTM D955 |
Hardness |
Nominal Value
|
Unit
|
Test Method
|
Rockwell Hardness (R-Scale, 23°C, Injection Molded)
|
110
|
ASTM D785 |
Mechanical |
Nominal Value
|
Unit
|
Test Method
|
Tensile Strength 3 (Yield, 23°C, 3.20 mm, Injection Molded)
|
50.0
|
MPa
|
ASTM D638 |
Tensile Elongation 3 (Break, 23°C, 3.20 mm, Injection Molded)
|
>10
|
%
|
ASTM D638 |
Flexural Modulus 4 (23°C, 6.40 mm, Injection Molded)
|
2550
|
MPa
|
ASTM D790 |
Flexural Strength 4 (23°C, 6.40 mm, Injection Molded)
|
82.0
|
MPa
|
ASTM D790 |
Impact |
Nominal Value
|
Unit
|
Test Method
|
Notched Izod Impact
|
ASTM D256 | ||
23°C, 3.20 mm, Injection Molded
|
270
|
J/m
|
|
23°C, 6.40 mm, Injection Molded
|
220
|
J/m
|
Thermal |
Nominal Value
|
Unit
|
Test Method
|
Deflection Temperature Under Load 5 (1.8 MPa, Unannealed, 6.40 mm, Injection Molded)
|
85.0
|
°C
|
ASTM D648 |
Vicat Softening Temperature
|
93.0
|
°C
|
ASTM D1525 |
available quantity 16 tons